Polycrystalline diamond and manufacturing method thereof

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 9878914
SERIAL NO

15131971

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

Nano polycrystalline diamond is composed of carbon and a plurality of impurities other than carbon. A concentration of each of the plurality of impurities is not higher than 0.01 mass %, and the nano polycrystalline diamond has a crystal grain size (a maximum length) not greater than 500 nm. The nano polycrystalline diamond can be fabricated by preparing graphite in which a concentration of an impurity is not higher than 0.01 mass % and converting graphite to diamond by applying an ultra-high pressure and a high temperature to graphite.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
SUMITOMO ELECTRIC INDUSTRIES LTDOSAKA-SHI OSAKA 541-0041

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Ikeda, Kazuhiro Itami, JP 65 219
Sumiya, Hitoshi Itami, JP 92 583
Yamamoto, Katsuko Itami, JP 30 122

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation

Maintenance Fees

Fee Large entity fee small entity fee micro entity fee due date
7.5 Year Payment $3600.00 $1800.00 $900.00 Jul 30, 2025
11.5 Year Payment $7400.00 $3700.00 $1850.00 Jul 30, 2029
Fee Large entity fee small entity fee micro entity fee
Surcharge - 7.5 year - Late payment within 6 months $160.00 $80.00 $40.00
Surcharge - 11.5 year - Late payment within 6 months $160.00 $80.00 $40.00
Surcharge after expiration - Late payment is unavoidable $700.00 $350.00 $175.00
Surcharge after expiration - Late payment is unintentional $1,640.00 $820.00 $410.00