Grain refinement, aluminium foundry alloys

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 9371573
APP PUB NO 20150082947A1
SERIAL NO

14358726

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

The present invention describes an effective grain refining practice for aluminum foundry alloys. The method described herein relies on the control of the Titanium level of the alloy to be grain refined and the addition of boron once it is melted. Boron addition can be made via Al—B master alloys as well as with boron compounds such as KBF4 salt. The boron added into the melt dissolves first and then forms the AlB2 particles that act as potent substrates for the nucleation of aluminum once solidification process starts. The Ti concentration of the alloy must be controlled below 100 ppm for this method to offer effective grain refinement. The boron becomes ineffective when the Ti concentration in the alloy is higher.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
TUBITAK06100 ANKARA

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Alageyik, Fahri Kocaeli, TR 2 0
Birol, Yucel Kocaeli, TR 4 10
Cakir, Osman Kocaeli, TR 3 10

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation

Maintenance Fees

Fee Large entity fee small entity fee micro entity fee due date
11.5 Year Payment $7400.00 $3700.00 $1850.00 Dec 21, 2027
Fee Large entity fee small entity fee micro entity fee
Surcharge - 11.5 year - Late payment within 6 months $160.00 $80.00 $40.00
Surcharge after expiration - Late payment is unavoidable $700.00 $350.00 $175.00
Surcharge after expiration - Late payment is unintentional $1,640.00 $820.00 $410.00