According to this production method, the water content of a mixture of a chromium oxide (Cr2O3) powder and a sodium carbonate (Na2CO3) powder is brought to 1000 ppm or less, and the mixture is heated in an inert gas atmosphere at a calcination temperature (850 DEG C.) where the sodium carbonate and the chromium oxide undergo a calcination reaction. Sodium chromite is thereby obtained.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
SUMITOMO ELECTRIC INDUSTRIES LTDOSAKA JAPAN OSAKA

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Fukunaga, Atsushi Osaka, JP 125 399
Inazawa, Shinji Osaka, JP 104 675
Majima, Masatoshi Osaka, JP 169 532
Nitta, Koji Osaka, JP 166 415
Sakai, Shoichiro Osaka, JP 98 243

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation

Maintenance Fees

Fee Large entity fee small entity fee micro entity fee due date
11.5 Year Payment $7400.00 $3700.00 $1850.00 Apr 27, 2027
Fee Large entity fee small entity fee micro entity fee
Surcharge - 11.5 year - Late payment within 6 months $160.00 $80.00 $40.00
Surcharge after expiration - Late payment is unavoidable $700.00 $350.00 $175.00
Surcharge after expiration - Late payment is unintentional $1,640.00 $820.00 $410.00