Method for lithium predoping, method for producing electrodes, and electric energy storage device using these methods

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 9147876
APP PUB NO 20130284988A1
SERIAL NO

13763879

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

A predoping technique considered as highly practicable is an electrochemical method in which predoping is performed by assembling a battery such that an active material (electrode) and lithium are brought into direct contact with each other or short-circuited therebetween via an electric circuit, and by filling an electrolytic solution in the battery. However, in this case, much time is required, and there are problems such as the handling and the thickness accuracy of an extremely thin lithium metal foil that is not greater than 30 μm thick. By mixing a lithium-dopable material and lithium metal together in the presence of a solvent, such problems can be solved.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
KRI INCKYOTO JAPAN KYOTO

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Fujii, Masanori Kyoto, JP 41 155
Kinoshita, Hajime Kyoto, JP 19 261
Satake, Hisashi Kyoto, JP 2 19
Yata, Shizukuni Kako-gun, JP 15 270

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation

Maintenance Fees

Fee Large entity fee small entity fee micro entity fee due date
11.5 Year Payment $7400.00 $3700.00 $1850.00 Mar 29, 2027
Fee Large entity fee small entity fee micro entity fee
Surcharge - 11.5 year - Late payment within 6 months $160.00 $80.00 $40.00
Surcharge after expiration - Late payment is unavoidable $700.00 $350.00 $175.00
Surcharge after expiration - Late payment is unintentional $1,640.00 $820.00 $410.00