Iron-nickel alloy with a high level of ductility and a low expansion coefficient

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 8889066
SERIAL NO

12312935

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

The invention relates to a solid-solution strengthened iron-nickel alloy with a high level of ductility and an expansion coefficient <5×10−6/K in the temperature range between room temperature and −200° C. Said alloy consists of (in wt. %): between 0.005 and 0.05% of C; <0.02% of S; between 1 and 2% of Cr; between 35 and 38% of Ni; between 0.3 and 1.5% of Mn; <0.5% of Si; between 1.0 and 3.5% of ΣMo+W; between 0.2 and 1.0% of Ti; between 0.2 and 1.0% of Nb; <0.02% of P; and between 1.0 and 4.0% of Co; Fe constituting the remainder, in addition to production-related impurities.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
OUTOKUMPU VDM GMBH58791 WERDOHL

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
De, Boer Bernd Altena, DE 5 14
Hoberg, Bernd Werdohl, DE 1 1

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation

Maintenance Fees

Fee Large entity fee small entity fee micro entity fee due date
11.5 Year Payment $7400.00 $3700.00 $1850.00 May 18, 2026
Fee Large entity fee small entity fee micro entity fee
Surcharge - 11.5 year - Late payment within 6 months $160.00 $80.00 $40.00
Surcharge after expiration - Late payment is unavoidable $700.00 $350.00 $175.00
Surcharge after expiration - Late payment is unintentional $1,640.00 $820.00 $410.00