Glass-ceramics and method for manufacturing the same

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 7943539
APP PUB NO 20090042710A1
SERIAL NO

11815082

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

/° C. or below within a temperature range of 0° C. to 50° C. These glass-ceramics are manufactured by a step of melting glass raw materials, a step of forming the molten glass, a step of annealing the formed glass, a first heat treating step for heat treating the annealed glass at a temperature of 650-750° C. for 0.1 hour to 200 hours, and a second heat treating step for heat treating the glass at a temperature of 800-1000° C. for 0.1 hour to 50 hours.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
KABUSHIKI KAISHA OHARA15-30 OYAMA 1-CHOME SAGAMIHARA-SHI KANAGAWA 229-1186

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Minamikawa, Hiroyuki Machida, JP 6 38