Method of an ultra-short femtosecond pulse and KW class high average-power laser for preventing cold-worked stress corrosion cracking in iron steels and alloyed steels including stainless steels

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 7651576
SERIAL NO

11214044

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

The method of preventing cold-worked stress corrosion cracking in the iron steels and alloyed steels including stainless steels comprises removing a residual tensile stressed layer, optionally generating residual compression, through the impact of irradiation with the ultra-short femtosecond pulse and kW class high average-power laser, and removing a hardened surface layer extremely susceptible to stress corrosion cracking, whereby this susceptible hardened surface layer with many concentrated dislocation defects and the likes is removed without generating or introducing any of such hardened layer in the process of its removal. The method is free from the risk of damaging other equipment by peening with steel balls or other shaped shots, is almost unlimited in actual environment, effectiveness, work, place and other conditions for application, is inexpensive, and functions continuously for a much longer period than an ordinary nuclear reactor's service lifetimes.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
JAPAN ATOMIC ENERGY RESEARCH INSTITUTE2-2 UCHISAIWAI-CHO 2-CHOME CHIYODA-KU TOKYO

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Minehara, Eisuke Soraku-gun, JP 7 34
Nishimura, Akihiko Soraku-gun, JP 18 121
Tsukada, Takashi Soraku-gun, JP 23 135

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation