Method for heat-treating profiled rolling stock

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 6770155
APP PUB NO 20020134472A1
SERIAL NO

10075398

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

A process for the manufacture of a railroad rail of a steel alloy having a pearlitic microstructure. The rail is is shaped at a reduction rate of 1.8 to 8% and aligned straight in its longitudinal direction at a temperature between 770.degree. C. and 1050.degree. C., whereafter it is mounted with the head down and is allowed to cool slowly in still air to a temperature of 5 to 120.degree. C. above the Ar.sub.3 temperature, and upon reaching this temperature at least the rail head is dipped into a cooling liquid and is cooled to the temperature of conversion of an austenitic grain microstructure into a fine pearlitic grain microstructure.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
VOESTALPINE SCHIENEN GMBHKERPELYSTRASSE 199 LEOBEN 8700

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Moser, Alfred Leoben, AT 10 19
Pointner, Peter Leoben, AT 8 24
Prskawetz, Georg Leoben, AT 5 10

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation