Abstract

See full text

A hydrometallurgical process is provided for leaching nickeliferous laterite ores at temperatures below the boiling point of the pulp and at atmospheric pressure. The high iron fraction of the laterite, referred to as limonite, is first contacted with concentrated sulfuric acid to partially or completely dissolve the iron and nickel into solution. A reducing agent is used to keep the redox potential in solution below 1000 mV to enhance cobalt dissolution and more advantageously between 1000 and 900 mV to avoid reduction of ferric iron. Further mixing of the leach slurry in the presence of sodium, potassium, or ammonium allows formation of iron jarosite at ambient pressure. The resulting acid from iron hydrolysis is neutralized with the low iron fraction of the laterite ore (saprolite), thereby dissolving nickel into solution. The resulting final leach slurry can then be treated with conventional methods to recover nickel and cobalt from solution.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
CERRO MATOSO SABOGOTÁ

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Arroyo, J Carlos Allen, TX 3 25
Neudorf, David A Blackrock, AU 6 57

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation