A method of producing a ultra fine grain steel made of ferrite having a mean grain size of not larger that 3 .mu.m as the base phase, after ingoting raw materials, by austenitizing the ingot by heating it to a temperature of at least an Ac 3 point, then, applying compression working of a reduction ratio of at least 50% at a temperature of from an Ae 3 point or lower to an Ar 3 point -150.degree. C., or at a temperature of at least 550.degree. C., and thereafter, cooling, wherein the strain rate as compression working is in the range of from 0.001 to 10/second.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
JAPAN AS REPRESENTED BY DIRECTOR GENERAL OF NATIONAL RESEARCH INSTITUTE FOR METALSIBARAKI

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Nagai, Kotobu Ibaraki, JP 28 90
Torizuka, Shiro Ibaraki, JP 25 48
Tsuzaki, Kaneaki Ibaraki, JP 16 156
Umezawa, Osamu Ibaraki, JP 3 11

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation