Tantalum (V) nitride pigments, process for the production thereof and use thereof

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 6235103
SERIAL NO

09510512

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

Tantalum(V) oxide may be nitrided with ammonia at 700 to 1250.degree. C. to yield tantalum(V) nitride. According to the invention, nitriding and consequently pigment quality are improved by adding at least one pulverulent oxide from the series SiO.sub.2, GeO.sub.2, SnO.sub.2, TiO.sub.2, ZrO.sub.2 and HfO.sub.2 or a pulverulent precursor of such an oxide in a quantity of at least 0.1 wt. %, calculated as oxide, to the tantalum(V) oxide to be nitrided and then nitriding the powder mixture.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
CERDEC AKTIENGESELLSCHAFT KERAMISCHE FARBEND-60327 FRANKFURT

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Letschert, Hans-Peter Hanau, DE 11 54
Voigt, Wilfried Rodenbach, DE 2 12

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation