Method of heat-treating a thin sheet coated with ZnAL by hot dip galvanization

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 6231695
SERIAL NO

09308104

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

A thin sheet is coated by hot dip galvanization with a zinc based alloy comprising 3.5% to 15% by weight of aluminum. Immediately after solidification of the coating, the thin sheet is heated for 2 to 10 seconds to a temperature 20 to 100.degree. C. above the melting point of the coating. The thin sheet is then cooled to room temperature.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
THYSSEN STAHL AGDUISBURG

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Durr, Wilhelm Dinslaken, DE 4 11
Heiler, Hans-Joachim Moers, DE 4 15
Hobelheinrich, Gunther Lennestadt, DE 1 2
Warnecke, Wilhelm Hamminkeln, DE 12 74

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation