Leather tanning process

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 5885302
SERIAL NO

08902594

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

The present invention refers to a new process meant for chrome and/or vegetable leather tanning. The process proposed by the invention comprises the steps of bating or purging, conditioning, and chrome and/or vegetable tannage. The conditioning step uses hydroxy-butaldehyde which reacts by blocking the amines of the collagen and releasing carboyxls. This reaction reduces the isoelectric point to 4.0-4.5, making the hide receptive or susceptible to effective chrome tannage by linking the carboxyls, or to tannin, by linking through hydrogen bridges. Hydroxy-butaldehyde is used in the conditioning step in a proportion of 2.5-3.0% as compared to the weight of the delimed hide, in a concentration of 40.+-.2%, with a pH of 4.2-4.4, and with the reaction time being from 3 to 4 hours.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
SETA S A -EXTRATIVA TANINO DE ACACIAESTANCIA VELHA RS

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Leuck, Carlos Alfredo Rio Grande do Sul, BR 1 4

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation