Method of retarding irradiated nuclear vessel crack initiation and extensions

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 5563927
SERIAL NO

08197892

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

An irradiated steel pressurized nuclear reactor pressure vessel 10 is provided with a crack initiation retarding and crack extension retarding reactor vessel integrity girdle 20 or 120 made up of shoes or links 22, with mechanical take up joints (26 to 34a or 126 to 134a). Instead of pivoted shoe links 22, the girdle 120 may be made using constricting roller chain links 122. In any event, crack initiation and crack extension which may result from pressure loading or vessel material embrittled in the beltline region by neutron bombardment is retarded by maintenance of a prestress under the nozzles during all periods of operation of the reactor.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
ABB COMBUSTION ENGINEERING NUCLEAR POWER INC9516-0402 2000 DAY HILL ROAD WINDSOR CT 06095

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Ayres, David J Canton Center, CT 2 25
Formanek, Frank J West Suffield, CT 13 203
Kendrick, Scott A Colchester, CT 16 574
Leombruni, Pete Wethersfield, CT 1 13
Margotta, Kenneth V Ellington, CT 8 75
Siegel, Edward A W. Hartford, CT 4 75

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation