Method for producing high opacifying kaolin pigment

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 5371051
SERIAL NO

08172552

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

A method for producing calcined kaolin pigments of high opacifying properties and low abrasion. A kaolin crude is selected having a G.E. brightness in the range of 70 to 80, a titania content of 2.0 to 3.0% by weight, less than 2% iron expressed as Fe.sub.2 O.sub.3, and a particle size distribution such that at least 88% by weight of the particles of said crude are of less than 2 .mu.m E.S.D.. The crude is blunged with water, and the resultant slurry degritted to form an aqueous slurry having at least 65% by weight solids. The slurry is centrifuged and a fraction recovered having over 65% solids, and in which at least 92% by weight of the particles are of less than 2 .mu.m. The recovered fraction is dried to less than 1% moisture, and pulverized to break up agglomerates. The pulverized fraction is then calcined by heating same to 1450.degree. to 1600.degree. F. after which the calcined kaolin is milled to yield a product having a G.E. brightness of 79 to 81 and an Einleiner abrasion of not mere than 2.5 mg wt loss.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
ECC INTERNATIONAL INC5775 PEACHTREE-DUNWOODY RD N E ATLANTA GA 31082

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Ginn, Michael W Wrightsville, GA 10 104
McNeely, R Brock Davisboro, GA 2 19
Pope, William H Sandersville, GA 6 121

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation