Method for decreasing energy consumption during refining of fiber material while maintaining capacity

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 5152871
SERIAL NO

07647507

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

The energy consumption of a cellulosic fibrous material refiner is significantly reduced, while the capacity is maintained by reducing grinding frequency while increasing the retention time and power amplitude (edge bar load). The grinding frequency is maintained between about 200-2,000 Hz, preferably between about 300-900 Hz. The retention time is more than a second, being increased at least about 100 times compared to conventional disk refiners. The power amplitude is at least doubled. Retention time is increased by greatly increasing the retention volume by removing the majority (at least about 90%) of the steam at approximately the area that it is generated, minimizing the number of cutting elements, and disposing the grinding surfaces of the refiner so that they define a volume of revolution (e.g. a frusto-conical or cylindrical volume).

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
KVAERNER PULPING TECHNOLOGIES ABSE-652 30 KARLSTAD

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Gullichsen, Jonan Sjundea, FI 1 2

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation