Process for manufacturing semi-finished products from sintered refractory metal alloys

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 5102474
SERIAL NO

07397456

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

In a process for manufacturing semi-finished products from sintered refractory metal alloys with a stacked microstructure, the sinter feed reshaped by at least 85% is subjected prior to recrystallization annealing to an intermediate annealing for at least 20 minutes at a temperature not less than 700.degree. C. and not greater than that at which no further recrystallization occurs. Following this intermediate annealing, the hot feed is deformed by a further 3% to 30%. The process makes it possible to manufacture semi-finished products with a good stacked microstructure and of substantially greater dimensions, or of the same dimensions and a substantially better stacked microstructure, than can be obtained with known manufacturing processes.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
SCHWARZKOPF TECHNOLOGIES CORPORATION A CORP OF MDBALTIMORE CITY MD

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Eck, Ralf Reutte, AT 9 276
Leichtfried, Gerhard Reutte, AT 25 154

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation