A process is taught for preparing a coal substitute of low ash level from a composite of coal, mineral matter and pyritic sulfur comprising comminuting the coal composite in an aqueous medium to a size range which promotes the liberation of the mineral matter; subjecting the resulting slurry to fines agglomeration in the presence of a water-insoluble bridging organic liquid; separating the agglomerates from the liquid phase containing the bulk of the mineral matter and a portion of the pyritic sulfur; treating the coal fines by stripping the organic liquid from the fines surface; and redispersing the fines in an aqueous medium having a surface active agent to yield a high solids coal fines slurry so to permit magnetic separation of residual pyritic sulfur and other magnetic mineral matter.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
EXPORTECH COMPANY INCNEW KENSINGTON PA

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Oder, Robin R Export, PA 18 513

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation