Processes for Making Propylene-Based Copolymers Having Broad CDs and MWDs

Number of patents in Portfolio can not be more than 2000

United States of America Patent

APP PUB NO 20250101149A1
SERIAL NO

18717135

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

Processes for making propylene-based copolymers having broad molecular weight distributions and broad comonomer distributions using a single tubular reactor. Processes for making a propylene-based copolymer can include introducing propylene and at least one other olefin comonomer to a tubular reactor to produce a propylene-based copolymer having a broad comonomer distribution, a Mw of about 10 kg/mol to about 2.000 kg/mol, and a MWD of about 2.0 to about 10.0. The tubular reactor can include one or more heat exchanger elements, preferably a spiral heat exchanger. Propylene-based copolymer compositions can include propylene derived units and at least one other comonomer derived units, wherein the copolymer compositions have a broad comonomer distribution, a Mw of about 10 kg/mol to about 2.000 kg/mol, and a MWD of about 2.0 to about 10.0. Such compositions can have broad orthogonal comonomer distributions.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
EXXONMOBIL TECHNOLOGY & ENGINEERING COMPANYANNANDALE NJ

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Dharmarajan, Narayanaswami Houston, US 35 105
Doufas, Antonios K Houston, US 46 1005
Jordahl, Stacy Webster, US 2 0
Ma, Rong Houston, US 36 139
Shi, Jun Houston, US 255 3204

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation