In an aspect, a method for reducing the molecular weight of a polyester comprises extruding a composition comprising a chain scission agent and a polyester in a molten state to form a modified polyester. The chain scission agent can comprise a C2-12 diol and can be present in an amount of 0.1 to 5 weight percent based on the total weight of the composition. The polyester can comprise a C2-12 alkyl phthalate polyester having a weight average molecular weight, Mwi, of 15,000 to 100,000 g/mol based on polystyrene standards. The modified polyester can have a weight average molecular weight, Mwf, of at least 5% less than the weight average molecular weight of the polyester.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

  • Owner owned or assignment not recorded

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Alive, Keshavaraja Evansville, US 14 229
Gallucci, Robert Russell Mt. Vernon, US 91 1014

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation