METHOD FOR RECYCLING IRON ORE TAILING AND USE THEREOF

Number of patents in Portfolio can not be more than 2000

United States of America

APP PUB NO 20250011900A1
SERIAL NO

18442527

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

Disclosed are a method for recycling an iron ore tailing and use thereof. The method includes: 1) conditioning the iron ore tailing to obtain a first slurry, adding water glass and a sodium oleate-associated substance sequentially to the first slurry to obtain a first mixture, and subjecting the first mixture to first flotation to obtain a mixed flotation foam product and a mixed flotation grit; 2) filtering the mixed flotation foam product to obtain a solid, drying, roasting at 400° C. to 650° C., and grinding to obtain a ground product; and 3) conditioning the ground product to obtain a second slurry, adding sodium sulfide, water glass, sodium alginate, hydroxamic acid, and terpenic oil sequentially to the second slurry to obtain a second mixture, and subjecting the second mixture to second flotation to obtain a rare earth concentrate and a rare earth tailing.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
BAOTOU RESEARCH INSTITUTE OF RARE EARTHSBAOTOU INNER MONGOLIA 014030

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Chen, Biao Baotou, CN 75 547
GUO, Chunlei Baotou, CN 14 244
Li, Na Baotou, CN 361 1146
Liu, Yanjiang Baotou, CN 2 3
Qin, Yufang Baotou, CN 2 0

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation