METHOD FOR PRODUCING AN ELECTRODEPOSITED COPPER FOIL FOR LITHIUM SECONDARY BATTERY

Number of patents in Portfolio can not be more than 2000

United States of America

APP PUB NO 20240392458A1
SERIAL NO

18695995

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

The invention relates to an electrodeposited copper foil and its manufacturing method. The copper foil has an as produced tensile strength above 52 kgf/mm2, presents tensile strength above 50 kgf/mm2 after 120 days at 35° C. and presents a recrystallization property under thermal stress. The copper foil is manufactured using an electrolyte comprising: copper at a concentration of at least 60 g/L; sulfuric acid at a concentration of at least 60 g/L; a halogen ion at a concentration of less than 2 mg/L; a thiourea-family electrolytic additive at a concentration between 0.001 mg/L and 0.1 mg/L; and a TOC in the electrolyte of less than 10 mg/L.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
CIRCUIT FOIL LUXEMBOURGZONE INDUSTRIELLE C SALZBAACH WILTZ L-9559

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
JACQMIN, Guillaume Bastogne, BE 1 0
ROZEIN, Pierre Vielsalm, BE 1 0
STREEL, Michel Houffalize, BE 10 45

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation