CHEMICALLY STRENGTHENED GLASS AND METHOD FOR MANUFACTURING SAME

Number of patents in Portfolio can not be more than 2000

United States of America

APP PUB NO 20240368032A1
SERIAL NO

18775847

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

A chemically strengthened glass has a thickness of more than 2 mm, a surface compressive stress CS0 of 400 MPa to 1200 MPa, a depth of compressive stress layer DOL-tail of 2.7 μm to 30.0 μm, an absolute value of an average slope of a stress profile from a surface to the DOL-tail of 20 MPa/μm to 500 MPa/μm, and a tensile stress CT of 1.0 MPa to 16 MPa.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
AGC INC5-1 MARUNOUCHI 1-CHOME CHIYODA-KU TOKYO 100-8405

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
FUJIWARA, Yusuke Tokyo, JP 110 937
KOBAYASHI, Yusuke Tokyo, JP 210 868
MORISHIMA, Yusuke Tokyo, JP 2 0
NAGASAKO, Takumi Tokyo, JP 7 68
OZEKI, Masao Tokyo, JP 40 744
TAKATO, Yoichi Tokyo, JP 3 0

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation