Chemically Strengthened Glass Ceramic, Preparation Method Thereof, and Electronic Device

Number of patents in Portfolio can not be more than 2000

United States of America Patent

APP PUB NO 20240300855A1
SERIAL NO

18263385

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

A chemically strengthened glass ceramic includes strengthening layers respectively formed on opposite sides, and each of the strengthening layers includes a potassium strengthening layer and a sodium strengthening layer sequentially located from a surface to an inside of the chemically strengthened glass ceramic. A depth of the potassium strengthening layer is 0.01 micrometers (μm) to 5 μm. A depth of the sodium strengthening layer is greater than or equal to 0.1t, where t is a thickness of the chemically strengthened glass ceramic. An average transmittance of a three-dimensional (3D) chemically strengthened glass ceramic in an optical wavelength range of 400 nanometers (nm) to 700 nm is greater than or equal to 85 percent %; a b value of a Lab color chromaticity indicator is greater than or equal to −2.0; and a haze is less than or equal to 0.25%.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
HUAWEI TECH CO LTDSHENZHEN GUANGDONG 518129

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Chen, Jiejie Shanghai, CN 1 1
Chen, Shifeng Shenzhen, CN 129 3346
Huang, Yihong Shanghai, CN 15 19
Lin, Geng Shanghai, CN 23 276
Xu, Wenbin Shenzhen, CN 31 84
Zeng, Zhou Shanghai, CN 1 1
Zhu, Guangxiang Shanghai, CN 3 2

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation