ASSOCIATIVE RHEOLOGY MODIFIER COMPOSITION AND METHODS FOR MAKING THEREOF

Number of patents in Portfolio can not be more than 2000

United States of America Patent

APP PUB NO 20220363922A1
SERIAL NO

17662674

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

An associative rheology modifier is obtained by coupling of a rheology modifier precursor with a coupling agent. The rheology modifier precursor is formed by reacting a rosin acid with a polyether at a mole ratio of the rosin acid to the polyether of >2:1, at a temperature from 180-350° C. and in the presence of an acid catalyst. The polyether has a molecular weight of 500-10,000 g/mol and the rheology modifier precursor has a water solubility of >10 wt. % concentration. The associative rheology modifier has a molecular weight (Mw) from 1500-25,000 g/mol. The associative rheology modifier shows a high shear thinning effect at low shear rate. A composition is also provided comprising the associative rheology modifier.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
KRATON POLYMERS LLCHOUSTON TX 77084

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Ding, Ruidong Houston, US 30 128
Reiter, Chad Savannah, US 7 1
Rucker, Donna Savannah, US 3 34
Tian, Jason Houston, US 21 76

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation