A method for formation of scorodite and for stabilization of arsenic by formation of scorodite, comprising using sodium hypochlorite as an oxidizing agent. The method comprises producing sodium hypochlorite having a concentration in a range between 1 and 3 w/w % using a diaphragm-less electrolytic cell operating with a sodium salt solution having a salt concentration in a range between 2 and 10 w/w %; diluting a sodium hypochlorite solution to less than 1 w/w % in an arsenic solution at an oxydo reduction potential in a range between 900 and 1100 mV (Pt, AgCl reference) and a pH comprised in range between 0.5 and 2.0; contacting a resulting oxidized arsenic with a ferric salt; and raising the pH to 5.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
DUNDEE SUSTAINABLE TECHNOLOGIES INC1002 SHERBROOKE STREET WEST SUITE 2060 MONTREAL H3A 3L6

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Barbaroux, Romain St-Joseph de Coleraine, CA 5 2
Lalancette, Jean-Marc Sherbrooke, CA 26 113
Lemieux, David Thetford Mines, CA 23 58

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation