A thermoelectric material is manufactured by a manufacturing process including annealing at an annealing temperature from 125° C. to 200° C. and for an annealing time from 5 minutes to 12 hours applied to a substance selected from the group consisting of conductive polymer, polystyrene sulfonate (PSS), tosylate (TOS), chloride and perchlorate and a substance as solvent selected from the group consisting of ethylene glycol, ethanol, dimethyl sulfoxide and isopropanol.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
NATIONAL INSTITUTE OF ADVANCED INDUSTRIAL SCIENCE AND TECHNOLOGYTOKYO TOKYO METROPOLIS

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Ishida, Takao Tsukuba-shi, JP 50 446
Mukaida, Masakazu Tsukuba-shi, JP 6 4
Naitoh, Yasuhisa Tsukuba-shi, JP 15 50
Wei, Qingshuo Tsukuba-shi, JP 3 0

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation