United States of America Patent

PATENT NO 9920397
SERIAL NO

14408124

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

A process for the removal of ferric iron as hematite from a nickel solution containing ferric and ferrous ions including the steps of: raising the temperature of the nickel solution to between 90° C. and the boiling point of the solution at atmospheric pressure; raising the pH of the nickel solution to be between 2 and 3; and adding a hematite seed to facilitate hematite precipitation, wherein ferric ions are precipitated as hematite in a predominantly crystalline form.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
CERRO MATOSO SABOGOTÁ

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Aguilar, Renato Antonio Loaiza Cordobo, CO 2 2
De, Hoyos Ruben Rangel Cordobo, CO 2 2
Liu, Houyuan Henderson, US 27 155
Rodríguez, Carolina Isabel Meneses Cordobo, CO 1 0

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation

Maintenance Fees

Fee Large entity fee small entity fee micro entity fee due date
7.5 Year Payment $3600.00 $1800.00 $900.00 Sep 20, 2025
11.5 Year Payment $7400.00 $3700.00 $1850.00 Sep 20, 2029
Fee Large entity fee small entity fee micro entity fee
Surcharge - 7.5 year - Late payment within 6 months $160.00 $80.00 $40.00
Surcharge - 11.5 year - Late payment within 6 months $160.00 $80.00 $40.00
Surcharge after expiration - Late payment is unavoidable $700.00 $350.00 $175.00
Surcharge after expiration - Late payment is unintentional $1,640.00 $820.00 $410.00