Abstract

See full text

A conductive thin film including a binder matrix and semiconductor nanowires dispersed therein is disclosed. The semiconductor nanowires are in the range of 30% to 50% by weight percentage of the thin film. The present invention also discloses a method of making such thin film. The method includes the steps of: mixing a plurality of semiconductor nanowires with a polymer binder to obtain a printing ink; thinning the printing ink with a solvent to achieve a predetermined viscosity; printing the printing ink on a substrate to form a conductive thin film thereon and evaporating the solvent at a rate slower than the evaporation rate of water.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
NANO AND ADVANCED MATERIALS INSTITUTE LIMITEDROOM 3641-3649 THE HONG KONG JOCKEY CLUB ENTERPRISE CENTER THE HONG KONG UNIVERSITY OF SCIENCE AND TECHNOLOGY HONG KONG

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
SUN, Caiming New Territories, HK 9 19

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation