METHOD FOR MANUFACTURING BIOACTIVE GLASS AND BIOACTIVE GLASS

Number of patents in Portfolio can not be more than 2000

United States of America Patent

APP PUB NO 20140348941A1
SERIAL NO

14073880

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

A method for manufacturing bioactive glass includes the steps below. A precursor and a polar solvent are mixed to form a mixed solution, in which the precursor includes a silicon precursor, a calcium precursor and a phosphorus precursor. The mixed solution is atomized to form a mixture droplet. The mixture droplet is oxidized in an environment of 500° C. to 900° C. to form the bioactive glass.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
NATIONAL TAIWAN UNIVERSITY OF SCIENCE AND TECHNOLOGYTAIPEI 106
TAIPEI MEDICAL UNIVERSITY (TMU)NO 250 WUXING ST XINYI DIST TAIPEI CITY 110

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
CHOU, Yu-Jen TAIPEI CITY, TW 6 12
LIN, Chung-Kwei TAIPEI CITY, TW 3 6
SHIH, Shao-Ju TAIPEI CITY, TW 5 17

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation