Abstract

See full text

A high Si-containing austenitic stainless steel having corrosion resistance in a nitric acid environment at a high temperature is made by hot-rolling a slab of stainless steel and heat treating the hot-rolled stainless steel at a temperature of 1100 to 1160° C. The steel is cooled at cooling rate of at least 100° C./min. The stainless steel has a chemical composition containing: C: at most 0.04%; Cr: 7 to 20%, Ni: 10 to 22%, Si: 2.5 to 7%, Mn: at most 10%, sol. Al: at most 0.03%, P: at most 0.03%, S: at most 0.03%; N: at most 0.035%, a total of one or more of Nb, Ti, Ta, and Zr being 0.05 to 0.7%; and the remainder Fe and impurities. The heating temperature during the hot rolling is Th in which ΔT of Formula (1): Th=1135−90Si−2.9Cr+40 Ni−ΔT is at least 30□C.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
NIPPON STEEL CORPORATION6-1 MARUNOUCHI 2-CHOME CHIYODA-KU TOKYO 1008071 ?1008071

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Kita, Hayato Joetsu-shi, JP 11 91
Shibuya, Masayuki Narashino-shi, JP 11 40
Sukawa, Tomoyuki Joetsu-shi, JP 2 0
Yoshida, Shuuji Joetsu-shi, JP 3 1

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation