Method for Producing a Hot-Rolled Flat Steel Product

Number of patents in Portfolio can not be more than 2000

United States of America Patent

APP PUB NO 20140007992A1
SERIAL NO

13978969

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

A method for generating a flat steel product comprising the steps of: melting a steel melt, comprising, in addition to Fe and unavoidable impurities (in wt %) C: 0.5-1.3%, Mn: 18-26%, Al: 5.9-11.5%, Si: <1%, Cr: <8%, Ni: <3%, Mo: <2%, N: <0.1%, B: <0.1%, Cu: <5%, Nb: <1%, Ti: <1%, V: <1%, Ca: <0.05%, Zr: <0.1%, P: <0.04%, S: <0.04%; casting the steel melt into a cast strip; heating the cast strip to an initial hot-rolling temperature of 1100-1300° C. at a heating rate of at least 20 K/s; hot rolling the cast strip into a hot strip; cooling the hot strip within 10 seconds after the hot rolling at a cooling rate of at least 100 K/s to <400° C.; and winding the cooled hot strip into a coil at a coiling temperature of up to 400° C.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
THYSSENKRUPP STEEL EUROPE AG47166 DUISBURG

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Balichev, Evgeny Dusseldorf, DE 4 11
Bian, Jian Koeln, DE 5 64
Hofmann, Harald Dortmund, DE 40 410

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation