TEMPERATURE STABLE CAST-IRON ALLOY AND ITS USE

Number of patents in Portfolio can not be more than 2000

United States of America Patent

APP PUB NO 20110042051A1
SERIAL NO

12377043

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

A description is given of a temperature-stable cast-iron alloy having high wear resistance at temperatures between 500 and 900° C. The alloy is characterized in that it has the following composition expressed in weight percentages: chromium: 15.0-20.0%, carbon: 1.0-2.0%, manganese: 1.5-2.0%, silicon: 0.8-1.2%, nickel: 8.0-10.0%, molybdenum: 0.8-1.2% balance iron and unavoidable metallic and non-metallic contaminants where the non-metallic contaminants comprise nitrogen, oxygen, phosphorous and sulphur. Hereby is obtained a cast-iron alloy which has a higher wear resistance and a reduced tendency to form the undesirable sigma phase when heated to temperatures between 500 and 900 ° C. as compared to the known allows.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
F L SMIDTH A/S2500 VALBY

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Karlsson, Asger Brondby Strand, DK 2 3
Kirkegaard, Stage Rasmus Holstebro, DK 2 2

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation