, a region between 0.3 mm and 3 mm from the crucible inner surface has an OH group concentration and an OH group concentration gradient which increase as a distance from the inner surface decreases, and decrease as a distance from the inner surface increases. The vitreous silica crucible can be manufactured by a process comprising the step of heating and melting silica powder deposited on an inner surface of a rotating mold to vitrify the silica powder, wherein vapor-containing air is introduced during or right after the melting, or the crucible is reheated, after the melting and cooling, under a vapor-containing environment.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
JAPAN SUPER QUARTZ CORPORATIONAKITA-SHI AKITA-KEN 010-0065

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Harada, Kazuhiro Akita, JP 68 2189
Sato, Tadahiro Akita, JP 38 214

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation