Method for reducing autogeneous shrinkage of super high strength concrete

Number of patents in Portfolio can not be more than 2000

United States of America Patent

APP PUB NO 20060144299A1
SERIAL NO

10563231

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

A method is provided for reducing autogenous shrinkage in ultra high-strength concrete in the blending of ultra high-strength concrete with a compression strength in excess of 100 N/mm.sup.2, comprising the steps of: replacing 30 vol. % or less of coarse aggregate with artificial lightweight aggregate, and blending in a expansive additive in the amount of 30 kg/m.sup.3 of concrete and/or a shrinkage reducing agent in the amount of 4 wt. % or less per unit weight of binder, and thereby bringing the amount of autogenous shrinkage at a curing age of 91 days to 0-600 .mu.m/m. The artificial lightweight aggregate used has water absorption of 5% or greater and 20% or less, a collapse load of 1000-2000 N and a bone-dry density of 1.4-2.0 g/cm.sup.3.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
KAJIMA CORPORATION3-1 MOTOAKASAKA 1-CHOME MINATO-KU TOKYO 1078388 JAPAN

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Hishiki, Yoshihiro Tokyo, JP 2 6
Ichinomiya, Toshimichi Tokyo, JP 3 7
Kasai, Hiroshi Tokyo, JP 31 191
Morita, Yukihiko Tokyo, JP 1 4
Taira, Yohei Tokyo, JP 4 5
Takada, Kazunori Tokyo, JP 34 712
Watanabe, Takahiro Tokyo, JP 232 2355
Yanai, Shuji Tokyo, JP 3 6

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation