Method for making positive grids and lead-acid and batteries using such grids

Number of patents in Portfolio can not be more than 2000

United States of America Patent

SERIAL NO

09998248

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

A method for making positive grids for lead-acid batteries from calcium-tin-silver lead-based alloys comprises casting an alloy strip and then rolling the strip at a temperature between about the solvus temperature and the peritectic temperature of the alloy, quenching the rolled strip, then, preferably, heat aging at a temperature of 200.degree. F. to 500.degree. F., and fabricating into the positive grid, such grids having enhanced mechanical and high temperature corrosion resistance characteristics.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
THE KEMEL GROUP INCORPORATED1250 S LOOP 360 STE 3-601 AUSTIN TX 78746

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Rao, Purushothama Aurora, IL 20 584

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation